Abbreviation |
Chemical Name |
ABA |
Acrylonitrile-Butadiene-Acrylate |
ABS |
Acrylonitrile-Butadiene-Styrene |
ABS / PC |
Acrylonitrile-Butadiene-Styrene / Polycarbonate |
ABS / PVC |
Acrylonitrile-Butadiene-Styrene / Polyvinylchloride |
ABS + PUR |
Acrylonitrile-Butadiene-Styrene + Polyurethane |
AC |
Acrylic Copolymer |
ACM |
Polyacrylate Acrylic Elastomer |
ACS |
Acrylonitrile-Chlorinated Ethylene-Styrene |
ADC |
Allyl Diglycol Carbonate (CR-39) |
AEM |
Acrylate Ethylene Elastomer |
AES |
Acrylonitrile-Ethylene-Propylene-Styrene |
AHEW |
Amine Hydrogen Equivalent Weight |
AIBN |
Azobisdisobutyronitrile (Free Radical Initiator) |
AMA |
Acrylate Maleic Anhydride Terpolymer |
AMMA |
Acrylonitrile-Methyl Methacrylate |
AN |
Acrylonitrile |
AO |
Antioxidant |
APET |
Amorphous Polyethylene Terephthalate |
APO |
Amorphous Polyolefin |
APP |
Atactic Polypropylene |
AS |
Acrylic-Styrene Copolymer |
ASA |
Acrylic-Styrene-Acrylonitrile Copolymer |
ASA+PC |
Acrylic-Styrene-Acrylonitrile + Polycarbonate |
ATH |
Aluminum Trihydrate |
ATRP |
Atom Transfer Radical Polymerization |
AU |
Polyester Urethane Elastomer |